Can I re-paint the substrate afterwards?
Providing that the dissolved paint residues have been completely washed off and the substrate has been given at least two weeks to thoroughly dry, then it is possible to re-paint.
In some cases it is advisable to neutralise the surface with Neutraliser N-20 before painting. It is advisable to use an alkali resistant primer before painting after the use of Kling Strip, Stripper 4-F and Stripper 4-A.